Investigations of silicon nano-crystal floating gate memories
Arvind Kumar, Jeffrey J. Welser, et al.
MRS Spring 2000
Measurements have been made to 5.2 kbar at 541°C of the simultaneous diffusion of Au195 and Zn65 in ordered AuZn alloys having nominal compositions of 49.0-, 50.0-, and 51.2-at.% Zn. The activation volumes ΔV obtained from these data are maximum at 50:50 composition and decrease on both sides of stoichiometry. The value of ΔV at 50:50 is approximately 8.5 ± 0.8 cm3/mole or 0.9 times the molar volume VM, which is of the correct magnitude for a vacancy mechanism. The activation volumes for the two constituents are equal to within the experimental accuracy. The results are discussed in terms of the correlated six-jump vacancy mechanism operative in these highly ordered alloys, and are related to vacancy-defect vis-à-vis antistructure-defect structures at off-stoichiometric compositions. © 1972 The American Physical Society.
Arvind Kumar, Jeffrey J. Welser, et al.
MRS Spring 2000
R.D. Murphy, R.O. Watts
Journal of Low Temperature Physics
Ranulfo Allen, John Baglin, et al.
J. Photopolym. Sci. Tech.
Sung Ho Kim, Oun-Ho Park, et al.
Small