Dry oxygen pressure at 500 atm is used to grow SiO2 films 103 nm thick on silicon at 80°C. The residual film stress, chemical etch rate, refractive index, and density of the pressure-oxide films is measured and compared with measurements of thermal oxide films prepared at 1 atm dry oxygen pressure. The high pressure/low temperature films exhibited higher refractive indexes, slower chemical etch rates, and higher measured densities compared to 1 atm thermal oxides prepared at 1000°C. These results are attributed to the lower oxidation temperature rather than the higher oxidation pressure of the pressure-oxide films. It is concluded that the formation of higher density SiO2 films is a specific result of low temperature processing. The use of high pressure oxidation provides a convenient technique to prepare the low temperature high density SiO2 films of sufficient thickness for further study. © 1980, The Electrochemical Society, Inc. All rights reserved.
Fernando Marianno, Wang Zhou, et al.
INFORMS 2021
J.A. Barker, D. Henderson, et al.
Molecular Physics
Mark W. Dowley
Solid State Communications
Michiel Sprik
Journal of Physics Condensed Matter